Sintered parts, obtained by powder metallurgy method are
competetive with products produced by traditional methods. It is
possible to obtain sintered materials of required properties by
correct choice of raw materials and technological process
parameters. Elements sintered of iron and steel are used, among
others, in automotive, engineering and aircraft industries, in
building engineering, etc.
STANDARDS: BN-76/0886-23, BN-76/0886-24, BN-76/0886-25
Chemical composition | |||||
Type of material | Composition [%] | ||||
Fe | C | Cu | Ni | Mo | |
Sintered iron | rest | Max. 0,29 | Max. 10 | - | - |
Sintered low-carbon steels | rest | 0,3 ÷ 0,59 | Max. 1,0 | - | - |
Mechanical properties | ||||
Type of material | Density [Mg/m3] | Rm [MPa] | A [%] | HB |
Sintered iron | 5,7 ÷ 6,5 | 59 ÷ 118 | Max. 2 | 30 ÷ 35 |
6,5 ÷ 7,4 | 177 ÷ 246 | 5 ÷ 10 | 40 ÷ 60 | |
Sintered low-carbon steels | 5,7 ÷ 6,5 | 78 ÷ 147 | Max. 1 | 35 ÷ 40 |
6,5 ÷ 7,4 | 196 ÷ 295 | 2 ÷ 7 | 45 ÷ 75 |
Materials of different technical parameters may be produced on customer's request.